MJ 3563 Cotton Twill: The Specification Behind a 250 GSM Work Trouser Cloth
MJ 3563 is a 250 GSM, 3/1 right-hand cotton twill at 150 cm cut width, stocked in 143 reactive-dyed shades at 300 m per colour, and it is the cloth to specify for trousers and uniforms, not for bags. The five numbers that define it - 250 GSM, 150 cm, 100% cotton, 143 shades, 300 m - are also the five lines that belong on the purchase order, because almost every dispute on a twill order turns out to be a specification dispute rather than a quality dispute. Stock shades ship in 7-10 days; FOB China port runs US $1.95-2.10 per metre depending on shade, packing and quantity. What follows is the specification we quote against, the three faults that come back from the wash, and the test method we use to put a number on each of them.
What MJ 3563 is, in five numbers
MJ 3563 is defined by five numbers, and all five belong on the purchase order: 250 GSM finished weight, 150 cm cut width, 100% cotton, 143 stock shade numbers and 300 m minimum per colour. None of them is a range. A buyer who writes “about 250 GSM” has left room for a 240 GSM substitute that wears thin at the knee inside a season.
The finished width is approximately 147 cm after finishing, so a marker built on 150 cm will not close. The cloth is woven three-up right-hand on our own looms, then desized, mercerised, piece-dyed in reactive colours and given a compressive shrink finish. It is held under MTQS-2026-000006, and every roll carries a batch test report so a claim traces back to cloth rather than to a carton.
| Property | Value | Condition |
|---|---|---|
| Article and weave | MJ 3563, 3/1 right-hand twill | Direction cannot be substituted after approval |
| Composition | 100% cotton | No blend tolerance |
| Finished weight | 250 GSM | Measured on finished cloth, not greige |
| Cut width | 150 cm (finished approx. 147 cm) | State the finished figure on the marker |
| Colour card | 143 numbers across five card pages | Piece-dyed stock; custom shades after lab dips |
| MOQ | 300 m per colour | Not 300 m split across shades |
| Lead time, stock shades | 7-10 days | MJ 3563 only; custom quoted after dips |
| FOB China port | US $1.95-2.10 per metre | Shade, packing and quantity set the exact figure |
In plain terms: 250 GSM at 150 cm, 100% cotton, 143 shades, 300 m per colour, 7-10 days for stock. Those are the numbers to copy into the order, and the sections below explain what each one controls.
250 GSM vs 280 GSM: choose by what the garment has to survive
Choose MJ 3563 at 250 GSM for garments that bend and MY 989 at 280 GSM for articles that carry a load; the 30 GSM difference matters less than the end use. This is the comparison buyers ask for most often, because the two cloths sit next to each other on our range and are easy to confuse on a specification sheet.
| Property | MJ 3563 cotton twill | MY 989 heavy canvas |
|---|---|---|
| Weight | 250 GSM | 280 GSM |
| Organisation | 3/1 twill, diagonal wale | Canvas, plain-faced and firm |
| Width | 150 cm cut width | 150 cm |
| Composition | 100% cotton | 100% cotton |
| Colour card | 143 numbers, five card pages | 55 colours |
| Hand | Drape, washable, holds a pressed crease | Stiff, needs breaking in |
| Best for | Work trousers, uniforms, chinos, aprons, light jackets | Bags, upholstery, heavy outerwear, reinforcement |
| MOQ | 300 m per colour | 300 m per colour |
The decision is not which cloth is better. A 250 GSM twill has enough body for a chino and enough drape to move with a knee; put the same cloth on a bag that takes point loads at the corners and it will crease and abrade early. A 280 GSM canvas is right for that bag and wrong for a trouser, where its stiffness restricts movement and slows the sewing line. If the garment is a work jacket with many small panels, the twill also costs yield because of the one-way cutting rule in the shading section below. For the 280 GSM end in full, see our heavy cotton twill canvas guide; that page and this one are meant to be read together before the weight is fixed.
Why 3/1 right-hand twill, and what 2/1 or 2/2 would change
A 3/1 construction is the reason this cloth is dense, firm and sharply diagonal, and the direction of that diagonal is not interchangeable between an approved sample and a delivered roll. In a 3/1 twill each warp end floats over three weft picks before passing under one, and the next end starts its float one pick later. That one-pick stagger builds the continuous diagonal; three quarters of the visible face is warp.
A 2/1 lifts less warp to the surface, so it is lighter in the hand and softer in drape - the classic chino cloth. A 2/2 is balanced front and back, sits flatter, and is the base for herringbone and cavalry twill where the pattern rather than abrasion resistance is the point. On a right-hand twill the line runs from lower left to upper right; a left-hand twill mirrors it. If a cutting room has laid a marker for right-hand and the mill delivers left-hand, the panels still sew, but the diagonal reverses at every seam. State “3/1 right-hand twill” on the order, not just “twill”.
100% cotton or 65/35 poly-cotton: the laundry decides
The composition line should be set by the wash regime, not by the price per metre. A 65/35 poly-cotton is cheaper, resists creasing, shrinks less and holds its shade through repeated industrial washing; a 100% cotton twill breathes, takes dye deeper, feels natural against the skin and breaks down without shedding microfibre, but it wrinkles and moves in the wash unless it has been compressed.
For a uniform programme washed fifty times, the blend earns its place. For a chino sold on hand and colour depth, the 100% cotton is the point of the garment. MJ 3563 is 100% cotton with no blend tolerance, and its residual shrinkage is held to 3 percent maximum after three washes by a compressive finish - the figure is only meaningful because the cloth is not a blend. A blend substitution changes both the shrinkage and the hand, which is why the PO line says 100% cotton rather than “cotton-rich”.
Residual shrinkage: the 3 percent line after three washes
The number to write on the order is 3 percent maximum in warp and weft after three washes, measured on finished cloth, method ISO 6330 / ISO 5077, reported per lot. Untreated cotton twill moves 5 to 8 percent in the warp after a hot wash and 2 to 4 percent in the weft, because the warp yarns were held under tension from the loom beam to the cloth roll and recover that stretch when wetted. On a 32-inch inseam, the top of that band is close to two inches - enough to turn a trouser into a cropped trouser.
Mechanical compression, the process behind the word sanforised, brings residual shrinkage to about 3 percent or below in both directions. MJ 3563 is mercerised and compressed, so 3 percent is the figure we work to. Two conditions matter as much as the number: measure on finished cloth rather than greige, and ask for the figure after three washes rather than one. A mill that measures on greige, or after a single wash, is not lying about the cloth so much as describing a different cloth.
Skew: 3 cm across 150 cm is already 1.1 degrees off square
Skew is a distance, not an angle: how far the weft has travelled away from perpendicular over a metre of width, and on a 150 cm cloth 3 cm of skew puts the weft roughly 1.1 degrees off square. That sounds trivial and is not. Over a trouser leg it becomes a seam that rotates, and rotation stays visible because it never settles down the way shrinkage does after the first wash.
Skew does not twist a garment by itself. It twists one when panels are cut square to the selvedge rather than square to the weft: a marker laid on a roll with 3 cm of skew produces panels whose grain line is correct at one edge and 3 cm out at the other, and sewing two of those together builds a bias into the seam. Hold 2 cm or less per metre of width, measured across the full width at head, middle and tail, with the AATCC 179 result after laundering attached. The mill controls loom tension, the weft straightener and relaxation time before rolling; the cutting room controls whether the marker follows the weft.
The test we run: 50 x 50 cm, 350 mm marks, three washes
This is the test we run on MJ 3563 lots, and it is written so a buying office can repeat it without a laboratory: one 50 x 50 cm cutting from the middle of the roll, three pairs of points 350 mm apart, conditioned four hours at 20 °C and 65 percent relative humidity, measured before and after three washes. It follows the logic of ISO 6330 / ISO 5077 and AATCC 179 without needing their equipment.
Mark the three pairs along the warp, the weft and the diagonal with a contrasting thread and a steel rule, not a tape measure. Condition the piece for four hours at 20 °C and 65 percent relative humidity before the first measurement, record each distance, then wash three times and measure again. Report shrinkage per direction and skew across the full width, per lot. We pair that with AQL 2.5 in-line inspection and a 4-point roll check under D65 lighting, and stamp the batch test report on every roll. That combination - one 50 x 50 cm cutting, three 350 mm marks, four hours of conditioning, three washes, one report per lot - is the number behind the 3 percent and 2 cm limits, and it is why we quote a limit rather than a promise.
Directional shading: one-way cutting is not optional on a 3/1 twill
Shading is not a dye-lot fault; it is a layout decision made after the cloth was delivered, and the mill cannot be held to a claim for it. A 3/1 twill lays its floats into a continuous diagonal of small parallel cylinders, and light reflects off those cylinders in a fan whose bright line moves with the viewing angle. Turn one panel 180 degrees and two pieces of the same roll read as two different shades.
The rule is that every panel in a garment is laid in the same direction and no panel is rotated to fit. On a plain weave this costs nothing; on a twill it costs yield, because a piece that could have been turned into a gap cannot be. There is one genuine mill-side version: if the diagonal reverses inside a single roll, the loom has faulted and the roll is not shippable - that one is ours. A four-point inspection on a rolling machine will find it, but will not find ordinary shading, because every metre passes under the same lights at the same angle and there is nothing to compare against.
Check it in five minutes before anything is cut. Cut two squares of about 30 cm from the same roll, lay them face up with one rotated 180 degrees against the other, butt the edges together and step back to look from the side under daylight. If a soft line appears where they meet, the cloth shades and the marker must carry a one-way rule. Put that rule in three places: on the purchase order, in the margin of the marker with an arrow, and in the tech pack next to the fabric note.
Which shades show shading, and which hide it
Shading scales with how much light comes back off the float rather than out of the body of the cloth, so it is predictable from the colour and the finish before a single metre is cut. Dark, high-lustre shades show it most; pale, matte and raised surfaces hide it.
| Shade or finish | How much it shades | Why |
|---|---|---|
| Navy, black, deep olive, burgundy | Most | Dark surface sends proportionally more light off the float |
| Mercerised mid-tones | Noticeable | Lustre sharpens the highlight along the diagonal |
| Sand, stone, ecru, pale grey | Slight | High body reflectance swamps the float highlight |
| Brushed or peach-finished surface | Almost none | The raised fibre diffuses the reflection |
For a uniform programme in navy or black, budget the one-way yield loss and say so in the tech pack before costing. For a sand chino, the same rule still applies but the visual risk is small; the rule is cheap to keep and expensive to break selectively.
143 stock numbers, five card pages, and how a lab dip is approved
MJ 3563 is piece-dyed in reactive colours across 143 stock numbers printed on five card pages, and colour is agreed on a physical lab dip, never on a screen. Reactive dyes bond chemically to the cellulose rather than sitting on it, which is why a reactive cotton twill holds its shade through washing and keeps a soft hand instead of the slightly stiff finish a pigment or sulphur dye leaves behind.
The trade-off is process cost, not performance: reactive dyeing uses more water and more careful rinsing, and it is the reason a deep navy costs more per metre than a pale sand. On the card, numbers 1 to 143 run from the workwear navies and greys at the low end to fashion shades from number 60 up. Send a Pantone TCX reference or a physical swatch for a custom shade, and the dip date is quoted with the stock position rather than guessed. Keep one dye lot per shade, with the lot number on each roll and no mixing of lots inside a single order.
MOQ 300 m per colour, FOB US $1.95-2.10, 7-10 days
The commercial terms are 300 m per colour, FOB China port US $1.95-2.10 per metre, and 7-10 days for stock shades - that lead time belongs to MJ 3563 specifically and is not a general twill promise. The exact FOB figure depends on shade, packing and quantity; deep shades and tight packing sit at the top of the band.
Custom shades are quoted after lab dips rather than against a published day count. T/T 30/70 is standard, with CFR and CIF on request; allow 2-3 business days for the transfer to be credited and one day for inspection before packing. A buyer planning a retail season should also work backwards from the 10-14 week purchasing lead and 8-10 week sea freight allowance used across our range - the 7-10 day mill lead is the shortest part of that chain, not the whole of it.
What goes on the purchase order
Eight lines on the purchase order replace a paragraph of correspondence later, because most disputes on a twill order are specification disputes dressed up as quality disputes. The cloth is what it says it is; the order never said what it needed to be.
| Item | What to state | Why it matters |
|---|---|---|
| Article and weave | MJ 3563, 3/1 right-hand twill, 250 GSM, 150 cm, one direction only | Direction cannot be substituted after approval |
| Composition | 100% cotton, no blend tolerance | A blend changes shrinkage and hand |
| Residual shrinkage | 3% max in warp and weft after three washes, finished cloth, ISO 6330 / ISO 5077, per lot | Stops the cropped-trouser claim |
| Skew | 2 cm or less per metre, head / middle / tail, AATCC 179 after laundering attached | Stops the twisted-leg claim |
| Dye lot | Single lot per shade, lot number on each roll, no lot mixing | Makes a claim traceable to cloth |
| Cutting direction | All panels one direction, no piece rotated | Shading is a layout decision, not a mill fault |
| Quantity | 300 m minimum per colour, not split across shades | Protects the dye lot and the price |
| Inspection | AQL 2.5 in-line, 4-point D65 roll check, batch report per roll | Fixes the acceptance standard before shipping |
Read together, the eight lines say: 250 GSM at 150 cm, 100% cotton, one direction, 3 percent and 2 cm limits, one dye lot per shade, 300 m per colour, and a batch report on every roll. That is the whole of the specification, and it fits on one page.
Inspection: AQL 2.5, a 4-point D65 roll check and a batch report on every roll
Every MJ 3563 roll leaves the mill with a batch test report, because a claim that cannot be traced to a lot cannot be settled. The cloth runs on our own 30 Lenado air-jet looms in Zhuji, Zhejiang, with warp and weft counts set for 250 GSM and a three-up construction so the diagonal stays crisp instead of washing out into a flat face.
After weaving, the greige goes through desizing, mercerising and piece dyeing, then a compressive shrink finish that takes residual shrinkage under 3 percent. Inspection follows the Mujia Textile Quality Standard MTQS-2026-000006: AQL 2.5 in-line, then a 4-point roll check under D65 lighting before packing. The four-point check finds holes, oil, slubs, broken picks and a reversed diagonal inside a roll; it does not find directional shading, which is why the 30 cm two-square test belongs in the cutting room rather than in the inspection report. What we control is one diagonal direction for the full length of every roll, a consistent shade within a dye lot, and a lot number stamped on every roll. What we do not control is how the marker is laid.
The three faults that come back from the wash
Almost every complaint on a cotton twill order traces back to one of three things - residual shrinkage, skew, or directional shading - and none of the three is visible on a sample card. All three are preventable at the specification stage, which is why the PO table above exists.
Residual shrinkage shows at the first wash when the hem comes up; hold 3 percent after three washes on finished cloth. Skew shows at the tenth wear when the side seam has travelled around the leg; hold 2 cm per metre and align the marker to the weft. Shading shows in the shop when two panels from the same roll read as two shades; cut one way and keep the rule on the marker. They share one root cause - cloth held under tension during weaving and finishing relaxing towards the state it wanted all along - but they have different owners, and the order should say which side carries which one.
When MY 989 is the correct answer instead
MY 989 at 280 GSM is the correct answer when the article carries a load rather than bends: bags, upholstery, heavy outerwear and reinforcement panels. Its 55-colour card is narrower than the 143 numbers on MJ 3563, and its hand is stiff enough to need breaking in, but that stiffness is exactly what a bag panel wants at the corners.
The reverse also holds. Putting 280 GSM canvas on a chino buys stiffness nobody asked for and slows the sewing line; putting 250 GSM twill on a load-bearing bag buys early creasing and abrasion. If the end use is genuinely between the two - a heavy apron, for instance - decide on the wash regime first: industrial laundering favours the firmer canvas, while a garment that has to press to a crease favours the twill. The full 280 GSM specification is in our heavy cotton twill canvas guide.
Frequently asked questions
Is 250 GSM heavy enough for work trousers?
Yes, at the light end of the band. 260 to 300 GSM is the usual band for work trousers and uniform bottoms; below 240 GSM the cloth wears thin at the knee and the seat within a season, and above 320 GSM it becomes stiff enough to restrict movement and slows the sewing line. MJ 3563 sits at 250 GSM and suits chinos, work trousers and chore jackets rather than heavy construction wear.
How much will MJ 3563 shrink after three washes?
3 percent maximum in warp and weft, measured on finished cloth, method ISO 6330 / ISO 5077, reported per lot. Untreated cotton twill moves 5 to 8 percent in the warp after a hot wash and 2 to 4 percent in the weft; MJ 3563 is mercerised and compressed, which brings residual shrinkage to about 3 percent or below. Ask for the figure after three washes, not one, and on finished cloth rather than greige.
What makes a trouser leg twist, and is it the mill's fault?
Skew, not shrinkage. A 150 cm cloth with 3 cm of skew has its weft running about 1.1 degrees off square, and a marker laid square to the selvedge rather than to the weft builds that offset into the seam. Hold 2 cm or less per metre of width measured at head, middle and tail, with the AATCC 179 result after laundering attached. The mill controls loom tension and relaxation time; the cutting room controls whether the marker follows the weft.
Why do two panels from the same roll look like different colours?
Because one panel was cut the other way round. A 3/1 twill reflects light off its diagonal floats differently depending on the viewing angle, so two pieces from the same roll read as two shades when one is rotated. Cut two squares of about 30 cm from the same roll, lay one 180 degrees against the other and look from the side under daylight: a soft line at the join confirms shading. It is a layout decision, not a dye-lot fault - unless the diagonal reverses within a single roll, which is a weaving fault and is ours.
Can I order 300 m split across several shades?
No. The minimum is 300 m per colour, not 300 m across an order. MJ 3563 is stocked in 143 reactive-dyed numbers across five card pages, and a custom shade is quoted after a physical lab dip with a Pantone TCX reference or a swatch. Keep one dye lot per shade, with the lot number on each roll and no lot mixing inside a single order.
Should I specify MJ 3563 or MY 989 for a bag?
MY 989, at 280 GSM with 55 colours. MJ 3563 is a 250 GSM 3/1 twill built for garments that move - work trousers, uniforms, chinos, aprons - and will crease and abrade early under the point loads a bag puts on its corners. MY 989 is the stiffer canvas intended for bags, upholstery and heavy outerwear. Both are 100% cotton at 150 cm and both carry a 300 m per colour minimum.
What test report comes with each roll?
A batch test report per roll, backed by AQL 2.5 in-line inspection and a 4-point roll check under D65 lighting under MTQS-2026-000006. The shrinkage and skew figures come from one 50 x 50 cm cutting from the middle of the roll, three pairs of points 350 mm apart, four hours of conditioning at 20 °C and 65 percent relative humidity, and three washes before re-measuring. The 4-point check finds a reversed diagonal inside a roll; it cannot find directional shading, which is why the 30 cm two-square test is done in the cutting room.
Where to go from here
Send the garment, the shade number and the quantity per colour. We will reply with the stock position, a lab dip date and an FOB price against your actual packing. Request a Quote
MJ 3563 Cotton Twill. Send the Garment, Get FOB.
Send the garment type, shade number and quantity per colour — we reply with stock position, lab dip date and an FOB price against your actual packing within 24 hours.
Send Your Garment Spec