Burnout Velvet vs Solid Velvet: What Actually Changes
Burnout Velvet vs Solid Velvet: What Actually Changes
Burnout velvet and solid velvet start from the same woven pile cloth, and the difference is that burnout removes fibre while solid velvet keeps all of it. A chemical paste is printed in the pattern, and where it sits, one of the two fibres in the blend is degraded and washed out, leaving only the other fibre as a semi-transparent ground. Solid velvet is dyed whole and keeps its full pile across the entire width.
That single fact explains almost every practical difference a buyer runs into: burnout is lighter per metre, its patterned areas are weaker and translucent, it is cheaper per metre but not necessarily per kilogram, and it must be ordered per design because each pattern is a separate print run. Everything below works through those consequences, plus the four checks that tell burnout apart from printed and embossed velvet — the three processes buyers most often confuse.
H2 · The difference in one table
| Solid-dyed velvet | Burnout (devoré) velvet | |
|---|---|---|
| Process | Dyed whole; full pile everywhere | Chemical paste printed in pattern; one fibre degraded and removed |
| Pile coverage | 100% of the surface | Pattern areas lose the pile; ground only |
| Weight | ~250 GSM (our MJ-VSL01) | 170–220 GSM (our MJ-VBR01) |
| Appearance | Even colour, even lustre | Pattern reads translucent against an opaque ground |
| Strength | Uniform | Pattern areas are weak — single-fibre ground |
| Price per metre | From USD 3.20 | From USD 3.10 |
| Price per kilogram | Lower | Higher — extra print and wash steps |
| MOQ | 300 m, any colour | 300 m per design |
| Colour / design range | 24 in stock + 40 on card | 73 designs |
| Ironing | Normal, low heat, cloth between | Avoid direct heat on pattern areas |
| Best for | Abaya, kaftan, structured dress, upholstery | Eveningwear, occasion wear, scarves, sheer-layer curtains |
H2 · What the process actually does
The cloth is a blend or interweave of two fibres with different chemical resistance. A print paste carrying the active agent is applied in the pattern. Where it sits, one fibre is broken down and removed in the washing that follows; the other fibre is unaffected and remains.
Two consequences follow directly, and they are the ones that matter commercially:
The cloth gets lighter. Fibre has been taken out. Our burnout line runs 170–220 GSM against 250 GSM for the solid, on a comparable base cloth. That is not a lighter base — it is the same base with material removed in the pattern.
The cloth gets weaker where the pattern sits. What remains in a pattern area is a single-fibre ground with no pile. It has far less mass and far fewer load paths than the surrounding cloth. This is inherent to the process, not a defect, and it dictates how the fabric must be cut and sewn.
We deliberately do not publish the specific chemistry, because the agent and its concentration are adjusted per base cloth and per design, and a number copied from another mill's recipe would be wrong for ours. What a buyer needs is the behaviour, not the recipe.
H2 · Why burnout is cheaper per metre but dearer per kilogram
This is the most common pricing confusion we see, and it is worth being blunt about.
Burnout carries more process steps than solid: printing the paste, the fixation stage, and the washing that removes the degraded fibre. It should cost more per unit of cloth. And it does — per kilogram.
But burnout weighs less per metre, because fibre has been removed. At 170–220 GSM against 250 GSM, the weight difference is roughly 12–32%. That is enough to pull the per-metre price below the solid line even though the per-kilogram cost is higher.
So compare on the number your costing actually uses. If you cost a garment per piece, per-metre is what matters and burnout can be the cheaper choice. If you cost by weight — which is normal for scarves, for freight calculations, and for any quote built on kilograms — burnout is the dearer cloth and quoting it as "cheaper" will lose you margin.
H2 · Why burnout is ordered per design
Each of our 73 burnout designs is a separate print run: a separate paste application, a separate fixation, a separate wash. There is no way to combine two designs into one run without doubling the setup.
That is why the minimum is 300 m per design, not 300 m in total across a mixed order. A buyer who wants six designs at 50 m each is asking for six print runs at one-sixth the minimum, and no mill can absorb that.
Solid velvet has no equivalent constraint. One dye lot covers the full 24 stock colours and the 40 card colours, and a 300 m order can be split across colours within reason. That flexibility is a real advantage of the solid line and is worth weighing against burnout's visual appeal.
H2 · Four checks that separate burnout from lookalikes
Buyers regularly receive printed or embossed velvet described as burnout. They are not the same thing and they behave differently in production.
1. Hold it to the light.
Burnout pattern areas are translucent — you can see light through the ground where the pile is gone. Printed velvet is opaque everywhere; the pattern is ink sitting on top of an intact pile.
2. Look at the reverse.
On burnout, the reverse of a pattern area shows the ground structure clearly, with a visible edge where the pile stops. On printed velvet the reverse is unaffected by the pattern.
3. Feel the pattern boundary.
Burnout has a physical step at the edge of a pattern — the pile ends and the ground begins. Printed velvet has no step; the surface is continuous. Embossed velvet has a step too, but it is a compressed pile rather than a removed one, and it recovers if you steam it.
4. Tear a corner off the sample.
Burnout pattern areas tear easily along the ground. Printed velvet tears like normal velvet. This is destructive — use the sample offcut, not the bulk.
A fifth check, if you have a balance: cut the same area from a burnout and a solid sample of the same width and weigh them. The burnout will be lighter by the amount of fibre removed.
H2 · The three processes, side by side
| What happens | Pile in pattern area | Translucent | Recovers when steamed | |
|---|---|---|---|---|
| Burnout / devoré | Fibre removed chemically | Gone | Yes | No — it is gone |
| Printed velvet | Ink applied on intact pile | Intact, coloured | No | n/a |
| Embossed velvet | Pile crushed by heated roller | Crushed flat | No | Yes — partly |
Only the first is burnout. If a supplier's "burnout" recovers when you steam it, it was embossed.
H2 · Our two woven lines
Both are woven warp-pile, 80% viscose / 20% nylon, no stretch. They are the same family of cloth; the difference is what has been done to it. (Woven vs knitted is a separate axis — see velvet vs velour.)
| MJ-VSL01 solid-dyed | MJ-VBR01 burnout | |
|---|---|---|
| Composition | 80% viscose / 20% nylon | 80% viscose / 20% nylon |
| Construction | Woven warp-pile | Woven warp-pile, pattern devoréd |
| GSM | ~250 | 170–220 |
| Width | 140 / 160 cm | 140 cm |
| Range | 24 in stock + 40 on card | 73 designs |
| MOQ | 300 m, any colour | 300 m per design |
| FOB | From USD 3.20/m | From USD 3.10/m |
Both are piece-dyed after weaving, not yarn-dyed — the colour goes through the cloth, which is why the pile and the ground match in the solid line and why burnout pattern areas take a slightly different depth of colour from the pile.
H2 · Which one to specify
Solid (MJ-VSL01) when:
- The garment is large and mostly plain — abaya, kaftan, dirac, wide-leg trouser
- You need uniform strength across the piece, especially for long seams and heavy wear
- You want to offer many colours from stock without a per-design minimum
- The end use is upholstery or curtain and needs dimensional stability
Burnout (MJ-VBR01) when:
- The design itself is the product — occasion wear, evening dress, sheer-layer overlay
- You want translucency as an effect: layered over a solid, or against light
- A scarf or shawl where the pattern carries the value
- Curtain where the pattern should read against daylight
Both, in one garment, is a normal and effective combination — burnout as the outer layer over a solid ground of the same colour family. That is a large part of why we keep both lines.
H2 · Production notes for burnout
Four things that go wrong, all of them avoidable.
Needle and stitch density. Pattern areas are single-fibre ground. Use a fine needle and a higher stitch density than you would on solid velvet, and avoid running a seam directly along a pattern boundary where the pile stops.
Do not over-handle the cut edges. Burnout frays more readily in pattern areas. Serge or bind early, and keep pattern areas away from the highest-stress points — armholes, crotch, waistband attachment.
Ironing. Direct heat on a pattern area can distort the ground. Press on the reverse, low heat, with a cloth between. Steam is safer than a hot plate.
Lining. Because pattern areas are translucent, the lining colour shows through. Match the lining to the ground, not to the pile, or the pattern will read as a different colour from the rest of the garment.
Frequently Asked Questions
Is burnout velvet weaker than solid velvet?
Yes, in the pattern areas only. The surrounding pile cloth is the same base and the same strength. A garment designed with the pattern away from stress points performs normally.
Why is burnout cheaper per metre if it has more process steps?
Because it weighs less. Fibre has been removed, so at 170–220 GSM against 250 GSM the per-metre price falls below the solid line even though the per-kilogram cost is higher. Compare on whichever unit your costing uses.
Can I mix designs to reach the 300 m minimum?
No. Each design is a separate print run. 300 m applies per design.
Can burnout be dyed to a specific Pantone?
The base can be dyed to a colour target, but pattern areas will read slightly different in depth because the pile is absent there. Send a physical standard and expect the pattern-to-ground relationship to be judged on the sample, not on a colour chip.
Is burnout the same as devoré?
Yes — same process, two names. "Devoré" is the French term used more in Europe, "burnout" more in the US and in export markets.
Can I get burnout on a stretch base?
Not from our woven lines. Burnout is done on our woven viscose/nylon base. If you need stretch plus a devoré look, that is a different development and we would quote it as such rather than substitute.