Why a burnout pattern is a process decision first

Buyers arrive at burnout velvet through a mood board. They have seen a devore gown with a rose vine running up one shoulder, or a leopard coat in a magazine, and they send the image with a price question. The mill answers with a pattern number, and the buyer assumes the hard part is done.

It is not. A printed pattern is an image applied to a cloth that already exists. A burnout pattern is a set of instructions about where the cloth should stop existing. The mill prints a chemical paste in the shape of the sheer areas, the paste destroys one fibre and leaves the other, and what remains is a cloth with holes in a designed arrangement. Every property of that arrangement — how wide the lines are, how close together, how much open area sits between motifs — is a process variable before it is an aesthetic one.

This is why two patterns that look equally beautiful on a screen can behave completely differently in production. One burns clean at the first attempt. The other comes back with a stiff rim around every motif, because the paste could not reach the viscose at the centre of a thin line, or the rinse could not carry the residue out of a tight corner. The buyer sees a quality problem. The mill sees a pattern that was drawn without the burn line in mind.

So the practical order of questions is: can this pattern be burned clean on this base cloth, at this width, in these colourways, with or without stones — and only then, do I like it. The rest of this guide works through those questions in that order.

What 80/20 viscose-nylon actually does when it burns

The base cloth behind every design in this guide is 80% viscose (rayon) and 20% nylon, at 170–220 GSM, on a usable width of about 140 cm. Those two fibres behave in opposite ways when the paste reaches them, and the whole craft depends on that difference.

The craft also has a structural precondition that is easy to miss: burnout is a woven process, not a knitted one. The paste has to sit on a stable ground while it works through the pile, which is why every design in this range is built on a woven base. A knitted velvet can be printed, brushed and crushed, but it cannot be burned into a sheer ground the way a woven one can — the loop structure does not survive the chemistry. If you are comparing velvet qualities for a burnout programme, that distinction is the first one to settle; it is covered in more detail in Woven vs Knitted Velvet.

Viscose is a regenerated cellulose. It does not melt — it carbonises and breaks down when attacked, which is what allows it to be destroyed in a controlled way rather than simply melting into the neighbouring fibre. Nylon is a polyamide. It resists the same chemistry and survives, which is why the sheer ground you see through is nylon mesh and not an empty gap.

Two consequences follow, and both matter commercially.

First, the pattern is a map of removed viscose, not an applied colour. There is no ink layer to crack, peel or fade off the surface, because there is no layer. This is why burnout velvet survives dry cleaning and gentle washing better than a surface-printed pile fabric — the design is structural.

Second, the sheer ground is a real cloth with real limits. Once the viscose is gone, what holds the motif in place is a nylon mesh that is a fraction of the original weight. A design that removes too much viscose in one area leaves a ground too weak to carry the garment's own weight at the shoulder or the hem. A design that removes too little reads as a textured solid rather than a burnout. The usable window between those two failures is narrower than most mood boards assume.

The 170–220 GSM band exists for the same reason. Below it, there is not enough viscose to remove and still leave a cloth with body. Above it, the paste has to travel further through the pile to reach the viscose, and the burn becomes less even across the width. The band is a process window, not a marketing range.

Line width: the number that decides whether a pattern burns clean

If you take one technical point from this guide, take this one: the width of the narrowest line in the motif decides more about the order than the size of the motif does.

The paste is printed onto the pile face. To burn, it has to travel down through the pile to the viscose ground, destroy it, and then be rinsed away along with the degraded fibre. In a broad open area, all three steps have room. In a line one or two millimetres wide, none of them do.

In our production experience, what goes wrong is specific and repeatable:

  • The paste cannot reach the base of a thin line. The burn stops partway, leaving a stiff, slightly darker rim where viscose survived. Under a light this reads as a hard edge, and on a garment it feels like a wire running through the cloth.
  • The rinse cannot clear a tight corner. Degraded viscose stays trapped where two thin lines meet, and it shows up later as a brownish or greyish smudge in the sheer area — the fault buyers most often mistake for dirt.
  • Registration drift shows up first on fine work. A fraction of a millimetre of misalignment is invisible on a broad motif and obvious on a hairline, because the sheer area has nowhere to hide.

This is the single most useful thing to look at when a buyer sends a design: not the overall composition, but the thinnest line in it, and the smallest gap between two motifs. Broad, open, well-spaced work is forgiving. Fine linear work and dense spacing are not, and no amount of sampling budget removes that.

In our experience, this is also why the designs in this range cluster where they do. The open florals and the animal textures are the easiest to run. The branch and sprig designs — which depend on thin, tapering lines — are the ones that need the most careful trial burn, and the ones where a first-order buyer is most likely to be disappointed by something that looked perfect on paper.

The sheer ground, and why multi-colour costs more than mono

Every design in this range is described as burnout on a sheer ground, and the ground is where the cost difference between a simple and a complex order hides.

After the burn, the sheer area is nylon mesh. It has a fixed openness determined by the weave, and it does not change colour the way the pile does, because there is far less fibre there to take dye. On a mono design — black-on-sheer, for instance — the pile is dark, the ground is a fine dark mesh, and the eye reads a single value with texture. Shade variation across the width is almost invisible, because there is nothing bright to compare it against.

On a multi-colour design, the ground and the motif separate. The motif takes colour strongly, the ground takes it weakly, and any unevenness in the dye penetration of that mesh becomes visible as a patchiness in the sheer areas specifically. The dyehouse is now being asked to make two different structures — pile and mesh — land on the same target shade, on the same roll, across 140 cm.

That is the real reason a multi-colour colourway costs more and takes longer to approve. It is not the dye cost of the extra colours. It is that each added colour is another chance for the sheer ground to read unevenly against the burned motifs, and the approval loop is where that gets caught.

The practical rule: if the garment already carries the look through cut, trim or embellishment, choose mono. The cloth does the texture and stays out of the way. If the cloth has to carry the look on its own — bridal, stage, ceremonial — multi-colour earns its cost, but budget for a longer approval.

The 73 designs, grouped by what they demand from the line

The thirteen designs detailed below are the ones most often specified. The full BR range now runs to seventy-one patterns, each with its own specification page. They share one base cloth — 80% viscose, 20% nylon, 170–220 GSM, about 140 cm usable, 300 m per colourway minimum, around 15 working days — and they differ in motif, colourway count, end use and, for three of them, whether a stone application runs on top.

The useful way to sort them is not by style but by how hard they are to burn. Three groups:

Group Designs What it asks of the burn line Best first order?
Open motifs
broad areas, generous spacing
BR-01 Rose Vine
BR-02 Peony Bloom
BR-06 Vintage Floral
BR-08 Leopard
BR-13 Stone Bold Floral
Forgiving. Paste reaches the base, rinse clears the open areas, registration drift hides inside the motif. Yes — start here
Mid-density
mixed broad and narrow, some tight spacing
BR-05 Paisley Damask Gold
BR-07 Yellow Blooms on Black Foliage
BR-09 Gravel Animal
BR-10 Chinese Foliage Trail
BR-11 Stone Butterfly
BR-12 Stone Leopard
Depends on the narrowest element. Ask for the trial burn before bulk on any of these. Second order
Fine linear
thin tapering lines, close spacing
BR-03 Pine & Coral Branch
BR-04 Abstract Branch
Hardest. Thin lines hold less paste, tight corners trap residue, drift is visible. Needs the most careful trial. Only after you have seen the line

The colourway counts are the second sort, because they drive the order value rather than the burn risk: BR-01 runs three colourways (lake blue, soft pink, rose-on-black), BR-03 and BR-06 five each, BR-04 seven, BR-02 is multi-colour on sheer, BR-05 is gold and champagne, BR-07 is a dark sprig on bright yellow, BR-08 is natural leopard tones, BR-09 is neutral multi-tone, BR-10 is black-on-sheer, and BR-11 and BR-12 are crystal work on black and coffee brown respectively, while BR-13 is a silver-sheen floral on yellow with no rhinestones at all.

Read the two sorts together and the decision usually makes itself. A first burnout order for a dress programme should start in the open group with a mono colourway. A bridal or ceremonial programme can justify the mid-density group with multi-colour, because the approval budget exists. The fine linear group is for buyers who already know how a particular mill's line behaves — which is a statement about experience, not about taste.

Mono-on-black against multi-colour: the colourway maths

Colourway count is where burnout orders most often exceed the budget the buyer had in mind, and the arithmetic is unforgiving because the minimum is per colourway, not per pattern and not per order.

At 300 metres per colourway, a single design in a single colourway is 300 metres. The same design in three colourways — which is what BR-01 offers as standard — is 900 metres. Two designs in one colourway each is 600 metres. A range of four designs in three colourways each is 3,600 metres, which is a different conversation with the finance team than the one the buyer thought they were having.

There are two honest ways to hold the number down.

Reduce colourways before reducing designs. A garment programme usually needs one or two colours far more than it needs four, and a single design in two colourways gives the sales team more usable range than two designs in one colourway, because the colour is what the customer actually chooses at the rail.

Use mono for the volume, multi-colour for the statement. Put the production colourway on a mono design, where the approval is short and the shade risk is low, and put the multi-colour on one hero piece. This is also how most of the buyers we work with actually structure a season, whether or not they describe it that way.

One more piece of arithmetic that catches people: the 300 metres is a minimum, not a target, and it is measured in metres of finished cloth at about 140 cm usable width. If your marker yields 1.8 metres per garment, 300 metres is roughly 166 garments in one colourway — fine for a boutique run, tight for a chain, and worth calculating before you promise a delivery date.

The two stone designs, the silver-sheen floral, and the temperature ceiling

Two designs in this range are not plain burnouts: BR-11 Stone Butterfly and BR-12 Stone Leopard both pair a burnout/devore ground with hot-fix rhinestone, and that second process changes what the cloth can survive. A third, BR-13 Stone Bold Floral, uses the word “stone” for its bold floral style but is a burnout with a silver-sheen floral rather than a rhinestone programme — do not plan a hot-fix press around it.

The sequence is fixed: the burnout runs first, because the ground has to exist before a stone can sit on it. Then a hot-fix application presses stones onto the burned cloth using a heat-activated adhesive. The adhesive is the constraint, and so is the nylon.

Nylon softens and melts in roughly the 215–220 °C range. Hot-fix adhesives are designed to activate well below that, which is exactly why the process is possible at all. But the margin is not large, and it narrows wherever the ground is thinnest, because a sheer area has almost no fibre mass to absorb and redistribute the heat that the press delivers. A stone placed on the open ground rather than on a pile motif is therefore the riskiest placement in the design — the one where a press that is slightly too hot or held slightly too long leaves a small, permanent distortion that reads as a dimple in the sheer.

Three practical consequences for a buyer:

  • Stone count and stone size drive the price more than the pattern does. The pattern is already on the line; the stones are added handling, an extra setting pass, and an adhesion check that a plain burnout never needs.
  • Ask where the stones sit relative to the ground. A design that clusters stones on pile motifs is more robust than one that scatters them across sheer areas, and that difference is not visible in a photograph.
  • Weight matters for drape. Stones add mass to a cloth whose sheer areas are already the weakest part of the structure. On a long gown or a dirac, that mass hangs from the thin ground, and a ground that was adequate for a plain burnout can start to distort under stones over a season of wear.

The two stone designs also tend to carry tighter colourway ranges than the plain ones — crystal on black, crystal on coffee brown — because every added colourway multiplies the work of matching stone tone to cloth tone. A crystal that reads right on black can read cheap on champagne. BR-13 sits outside that constraint: its silver sheen is part of the floral itself, so its colourway question is the ordinary dyeing one, not a stone-matching one.

Matching a pattern to the garment, not to the mood board

The single most reliable way to choose badly is to pick a pattern because it looks good as a flat image. Burnout behaves differently depending on how the cloth is cut, how much of it is in one piece, and how the garment moves.

What actually distinguishes the end uses is not formality but how much uninterrupted cloth the garment puts on show.

Garment What the cloth has to do Designs that fit
Evening gown, one-piece Carry the whole look across a large uninterrupted panel. The pattern is read at distance and in motion. BR-01, BR-02, BR-10
Somali dirac, Sudanese toub Long, loose, layered. The sheer ground does the work at the hem and sleeve; the motif reads at the shoulder and border. BR-05, BR-01
Qipao / cheongsam Close-fitting, short repeat, high contrast against skin. A dark ground with a defined motif reads best. BR-10
Abaya, kaftan Large flat panels, often over another layer. The pattern has to read through movement without competing with the underlayer. BR-03, BR-04, BR-07, BR-09
Bridal, stage, ceremonial The cloth is the product. Multi-colour and stone work earn their cost because nothing else is carrying the look. BR-02, BR-05, BR-13
Party dress, African occasion wear Bright ground, strong motif, stones acceptable. Short garment life per season, so maximum visual impact per metre. BR-11, BR-12, BR-13
Jacket, structured outerwear Needs body as well as pattern. The top of the 170–220 GSM band, and motifs that survive being cut into panels. BR-08, BR-09

Two rules sit underneath that table and are worth stating separately.

The bigger the uninterrupted panel, the more the pattern has to work at scale. A motif that reads as delicate on an A4 swatch can read as sparse on a full gown skirt, because the eye now has two metres of cloth to scan instead of twenty centimetres. Open, larger motifs survive scale-up. Fine linear work that looked exquisite in the hand can disappear into texture at three metres.

The more the garment is cut into panels, the more the pattern has to survive seams. Every seam interrupts the repeat, and on a sheer ground the interruption is visible because the mesh density changes at the join. Garments built from many small panels — structured jackets, panelled bodices — are better served by motifs that read as texture than by motifs that read as a single drawn image.

What 300 metres per colourway means across a range

The minimum is per colourway, and the colourway maths is in the section above. What buyers underestimate is the range-planning consequence: the minimum does not scale down when you spread across designs, it scales up.

A range of three designs in two colourways each is six minimums: 1,800 metres. A range of two designs in four colourways each is eight minimums: 2,400 metres — more cloth, from fewer designs. This is the opposite of how most buyers intuitively plan a collection, where adding designs feels like adding risk and adding colours feels like adding choice.

The arithmetic is the same one that governs velvet generally, and the reason it feels harsher on burnout is that a pattern is harder to substitute mid-season than a plain shade. The general structure of velvet minimums is set out in Velvet MOQ Explained.

For a first burnout season, the shape that works most often is: one open-motif design in two colourways as the volume piece, plus one mid-density design in a single colourway as the statement piece. That is 900 metres, three minimums, one design in the forgiving group and one in the group that needs a trial burn — enough range to sell from, small enough to survive a slow sell-through.

Worth knowing before you plan: at about 140 cm usable width, and with a typical gown marker yielding somewhere near 1.8 to 2.2 metres per garment depending on size and cut, 300 metres is roughly 140 to 165 garments. A three-design, six-colourway range at 1,800 metres is over 800 garments. If the plan is a boutique run, the range is already larger than the plan.

A4 swatches: three checks in five minutes

Swatches ship on request, and a swatch is not a colour card. It is the only chance to judge the burn before you commit, so it is worth knowing what to do with one.

Check one: hold it against a window. Look at the sheer areas specifically, not the motifs. The nylon mesh should read even — the same openness across the swatch, no patch where it is denser or thinner. Unevenness here is the fault that later shows up as blotchiness on a garment, and it is nearly invisible under office lighting. Daylight through the cloth is the test.

Check two: run a fingernail along the edge of a motif. A clean burn has a soft transition from pile to mesh. An incomplete burn has a stiff rim — a slightly raised, slightly harder line where viscose survived. This is the single fastest way to tell a well-run burn from a marginal one, and it takes seconds.

Check three: stretch the sheer area gently across the diagonal. The mesh should give and recover. If it goes slack and stays slack, or if a motif edge starts to separate, the burn removed too much viscose in that area and the ground is weaker than the design assumes. On a stone design, do the same check around a stone cluster.

What a swatch cannot tell you: how the colour will read at garment scale, how the ground behaves after ten washes, and how the pattern sits across a seam. Those need a trial burn and a wash test, which is the next section.

The four faults that only happen on burnout

Burnout has its own failure modes, and none of them appear on a solid velvet inspection sheet. Knowing the four is most of the difference between a useful inspection and a wasted one.

1. Incomplete burn. Viscose survives where it should have been removed, leaving a stiff rim or a dull patch. Causes: paste not reaching the base of a thin line, insufficient dwell time, or a base cloth at the top of the weight band. Visible under raking light, and tactile before it is visible — run a hand across the face.

2. Over-burn. The burn goes past the viscose into the ground, leaving a thin spot, a small hole, or a motif whose edge has lost definition. Causes: excess paste, too long a dwell, or a design that removes too much viscose in one area. Under tension this reads as a weak point, and it is where a garment will fail first.

3. Repeat misregistration. The pattern does not line up where the print repeat joins, so a motif is cut and re-started a few millimetres off. Invisible on a swatch, obvious on a full panel, and unfixable downstream. On fine linear designs this is the fault that ruins the most cloth.

4. Ground shading. The sheer areas read unevenly in colour — a patchiness that follows no pattern and does not wash out. Causes: residue trapped in the mesh during rinsing, or uneven dye penetration where the mesh and the pile have to reach the same shade. Worst on light and mid-tone multi-colour grounds, mildest on black-on-sheer.

There is a fifth thing that gets called a fault and is not: a faint tonal difference between the motif and the ground on a mono design, where the ground is slightly lighter because there is less fibre there to take dye. That is the structure showing through, not a defect, and it is worth saying so to a QC team before they write it up.

Inspection: what to look for on a burnout roll

A burnout roll needs a different inspection routine from a solid velvet roll, and the differences are all in how you use light and tension.

Inspect on the roll, in raking light, before cutting. The two faults that matter most — incomplete burn and over-burn — are close to invisible in flat diffuse light and obvious when light comes across the surface at a low angle. Set the light low and to one side. This is the whole reason burnout inspections fail: they are run under the same lighting as a solid fabric inspection, where these faults do not exist.

Check the repeat join at least once per roll. Walk the length and find where the print repeat meets itself. Look for a motif that is cut short or doubled. On a fine linear design, check two or three joins, not one, because misregistration can be intermittent.

Check the sheer ground against a light, in sections. Hold a section up and look through it. Patchiness in the mesh, or a residue haze, shows up immediately against a bright background and not at all against a dark one.

Do a tension check at the selvedge and at mid-width. The burned areas have less fibre, so the cloth behaves differently at the edges than in the centre. A ground that is sound mid-width can be noticeably weaker near the selvedge, where the burn and the finishing both concentrate.

For stone designs, add an adhesion check. Press a stone with a fingernail — it should not lift. Then look at the ground immediately around a stone cluster for any dimpling or glazing, which is the sign that the setting press ran too hot for the nylon beneath.

The cloth ships with a batch test report, and a 7-day uncut quality guarantee covers faults found before cutting. Both are worth using rather than filing: the guarantee exists precisely because burnout faults are hard to see and easy to discover too late.

Sampling and the 15-day lead time

Lead time on the ready designs runs about 15 working days, and it is worth understanding what that number does and does not include.

What it covers: the burn, the dyeing, the finishing and the packing of a colourway whose burn map already exists and has been run before. That is why a ready design is fast — the technical risk was taken out of it before you arrived.

What it does not cover: your approval loop, the swatch you have not yet looked at, and any change of mind about colourway. Those sit outside the 15 days and are usually where a delivery date actually slips.

The sequence that avoids surprises:

  1. Swatch first, always. A4 swatches ship on request, and the three checks in the section above take five minutes. Doing them before you place an order costs nothing and prevents most of the disappointment.
  2. Ask for a trial burn if the design is mid-density or fine linear. On open motifs the trial is usually unnecessary. On the branch and sprig designs it is the difference between a working order and a claim.
  3. Approve colourway against a physical swatch, not a screen. The sheer ground reads differently on every monitor, and a multi-colour ground is where screen-versus-cloth disagreement is largest.
  4. Wash a sample before bulk. Not because the cloth is expected to fail, but because you want to know how the ground behaves after washing while you still have leverage.
  5. Then confirm, and count the 15 working days from confirmation. Not from inquiry, not from sample request.

Payment terms on these designs run 30% with the order and 70% against documents, which is standard for made-to-order cloth and worth knowing before the finance conversation rather than during it.

Custom artwork: when to choose it over a ready design

Every design in this range exists because someone else already paid for the burn map. That is the entire value proposition of a ready design: the technical risk has been absorbed, and you are buying the output rather than the development.

Custom artwork is the right answer in three situations, and only those three:

  • You have a repeating programme. If the pattern will run for several seasons, owning it is worth the development cost, because a ready design is available to every other buyer of the same cloth.
  • The motif is the brand. Where the pattern is recognisably yours — a house signature, a licensed print — a stock design cannot substitute, regardless of how well it fits.
  • Nothing in the range fits the garment. Occasionally the geometry is wrong: the repeat is too large for a short garment, or the open areas land where the pattern needs to hold shape. Then a custom burn map is cheaper than forcing a stock design.

What custom artwork involves is a different clock, not a different craft: the design has to be converted into a burn map that respects the line-width limits described earlier, a trial burn has to confirm that the thinnest elements survive, and the first dye lot has to be approved before bulk. The development timeline for that process is covered separately in our guide to burnout pattern development, which walks the artwork-to-first-dye-lot route in detail.

The mistake to avoid is treating custom as a premium version of ready. It is not a better pattern; it is a longer project with a technical gate in the middle. If a ready design already fits the garment, custom adds time and cost without adding anything the customer will see.

Five mistakes that cost a burnout order

1. Choosing from a photograph and skipping the swatch. A burnout pattern is defined by what happens at the edge of every motif, and a photograph cannot show that. Every expensive burnout disappointment we see starts with a swatch that was never requested.

2. Ordering fine linear work as a first burnout. The branch and sprig designs are the most beautiful in the range and the least forgiving to run. A first order should be an open motif, so that when something goes wrong you know it is not the pattern.

3. Budgeting one minimum for a multi-colour range. The minimum is per colourway. A three-colourway order is three minimums, and the finance conversation is much easier before the order than after it.

4. Inspecting under office light. Incomplete burn and over-burn are raking-light faults. An inspection run under the same lighting as a solid fabric inspection will pass cloth that a garment maker will reject three weeks later.

5. Treating the sheer ground as decoration. The ground is a structural mesh carrying the garment's weight, and it is the weakest part of the cloth. A design that removes too much viscose for the garment's cut — particularly at a shoulder, a hem or a strap — will fail in wear, not in inspection, which is the most expensive place to find out.

The one-paragraph version

A burnout velvet pattern is a map of where the viscose was removed from an 80/20 viscose-nylon cloth, which makes every pattern a process decision before it is a design decision. The narrowest line in the motif decides whether the burn runs clean; broad open motifs are forgiving and fine linear work is not. Colourway count multiplies the minimum, because 300 metres applies per colourway and not per pattern. Multi-colour asks more of the dyehouse than mono, because the sheer ground and the pile have to land on the same shade. The two stone designs add a second process whose temperature ceiling is set by the nylon, so stones on sheer areas are the riskiest placement in any design. Thirteen designs in this range have their own specification page, all on the same base cloth at 170–220 GSM and about 140 cm usable, around 15 working days on a design whose burn map already exists. Request a swatch, hold it against a window, run a fingernail along a motif edge, stretch the ground across the diagonal — and if the design is mid-density or fine linear, ask for a trial burn before you commit. The pattern you can burn clean is worth more than the pattern you like most.

Frequently Asked Questions

What is a burnout velvet pattern?

It is a design burned into a two-fibre cloth rather than printed onto it. The cloth is woven from viscose and nylon, a chemical paste is printed where the sheer ground should be, and the paste destroys the viscose while the nylon survives. The pattern is therefore a map of where the viscose was removed, not an ink layer sitting on the surface.

Which pattern is easiest to burn clean?

Broad, open motifs with generous spacing burn cleanest, because the paste has room to reach the viscose and the rinse has room to carry the residue away. Fine linear work and tight spacing are the hardest, because a thin line holds less paste and leaves a stiff edge where the burn stopped short. If a design is your first burnout order, start with an open motif and move to fine work once you have seen how the mill's line behaves.

Can I order more than one pattern?

Yes, but each pattern carries its own minimum of 300 metres per colourway, and the minimums do not combine across patterns. Two patterns in one colourway is 600 metres, not 300. Three patterns in three colourways is 900 metres. Work out the total before you fall in love with a range.

Why do the stone designs cost more?

Because they are two processes, not one. The burnout runs first, then a hot-fix stone application runs over the burned cloth. The second pass adds handling, a setting temperature that has to stay below the point where the nylon ground is damaged, and an adhesion check that a plain burnout never needs. The stone designs also tend to carry fewer colourways, because each colourway multiplies the stone-matching work.

How do I choose between mono and multi-colour?

Choose mono when the garment is the product and the cloth is the ground: a black-on-sheer design reads as texture, hides shade variation and costs the least per colourway. Choose multi-colour when the pattern is the product: bridal, stage and ceremonial wear where the cloth has to carry the look on its own. Multi-colour asks more of the dyehouse because every added colour is another chance for the sheer ground to read unevenly against the burned motifs.

Can I use my own artwork instead of a ready design?

Yes, and for a repeating programme it is usually the right answer. Custom artwork runs on a different clock from a ready design: the design has to be converted to a burn map, a trial burn has to confirm the line widths survive, and the first dye lot has to be approved before bulk. A ready design skips all of that because the burn map already exists and has been run before.

The 13 Designs Detailed in This Guide